Gold Process Description 911 Metallurgist
With this flow configuration a large portion, approximately 70%, of the gold and silver dissolved in the grinding circuit will flow via the thickener overflow directly to the precipitation circuit. The four meter diameter x meter high leach tanks are sized for a total retention time of 48 hours at 45% solids.